JAGDISH METAL are leading and renowned exporter, stockiest and manufacturer of Aluminium Alloy 5082 Sheet & Plate in the market till date. Basically, aluminium alloy 5082 sheet and plates is aluminium magnesium alloy that gets hardened through cold work. It is not at all heat treatable to higher sheet and plate strength.

Aluminium Alloy 5083 Plates and Sheets is profoundly utilized as a part of marine applications because of its magnificent protection from general erosion. It has the most elevated quality of the non-warm treatable composites however isn't prescribed for use in temperatures over 65°C.
5083 Aluminium Sheet Temper 0, H32, H34, H38 as per ASTM B209, ASTM-B-209, EN573, and EN485 international standards. O, H111, or H112, UNS A95083, AMS-QQ-A-200/45083 AMS 4051 Plate, AMS 4051 7178-0 Alclad Plate, QQ-A-250/15 T0, 7178 A95083 Aluminium Plate 5083 Aluminium Plate ASTM B209, ASTM-B-209, EN573, and EN485 international standards.
| Standards | : | ASTM B209 / ASME SB209 |
| Temper | : | O, F, H12, H14, H16, H18, H19, H22, H24, H26, H32, H34, H36, H38, H111, H112, H321, T3, T4, T5, T6, T7, T351, T451, T651, T851 |
| Thickness | : | 0.2~300mm |
| Width | : | 500~2500mm |
| Length | : | 500~10000mm |
| Surface | : | Bright, polished, hair line, brush, sand blast, checkered, embossed, etching, etc. |
| Finish | : | Mill, Customer specific finish |
| Aluminium Sheet/ Plate Coating | : | PVC Coated, Color Coated, Polyester, Fluorocarbon, polyurethane and epoxy coating |
| Type | : | Hot-Rolled (HR) / Cold-Rolled (CR) Sheet / Plates/ Strips/ Coils/ Chequered Plates |
| Chemical Element | % Present |
|---|---|
| Aluminium (Al) | 95.2 to 98.3% |
| Chromium (Cr) | 0.25% max |
| Copper (Cu) | 0.1% max |
| Iron (Fe) | 0.5% max |
| Magnesium (Mg) | 0.6 to 1.2% |
| Manganese (Mn) | 0.4% to 1.0% |
| Silicon (Si) | 0.7 to 1.3% |
| Titanium (Ti) | 0.1% max |
| Zinc (Zn) | 0.2% max |
| Residuals | 0.15% max |
| Property | Value |
|---|---|
| Density | 2700 kg/m3 |
| Melting Point | 555°C |
| Modulus of Elasticity | 70 GPa |
| Electrical Resistivity | 0.038x10-6 Ω.m |
| Thermal Conductivity | 180 W/m.K |
| Thermal Expansion | 24x10-6 /K |
| Property | Value |
|---|---|
| Proof Stress | 85 Max MPa |
| Tensile Strength | 150 Max MPa |
| Hardness Brinell | 40 HB |